Back to Ganoksin | FAQ | Contact

Cleaning and Protecting Silver

I’ve enjoyed all the recent posts on this subject and have learned
about some great products, but (yes) there is even more. In my
websurfing I found a great article through the Soc.of American
Silversmiths. It has a strange title having to do with Cleaning
Silver with Toothpaste (!) yes/no, but actually goes into chemical
cleaners, electrolytic processes, abrasives, storage considerations,
and all the way down to cleaning your silver salt shaker’s corrosion.
You can find it at: www.silversmithing.com/care.html#Toothpaste.
Enjoy. Gary Strickland, GJG

If, for some strange reason, the link doesn’t work, just go to
www.silversmithing.com and scroll down the page to the heading
"Silver Care." You’ll see the Toothpaste article listed there.

Christine