 Hi Everyone! Does anyone know where we can buy PMC for the least
amount of money? I imagine like many things Rio is probably the
most expensive source. 

Thanks Laura Rio is the ONLY source. However, if you do enough of it
and become proficient, you can get certified to teach PMC work. That
takes 1/3 off the price for you at Rio Grande. You also can get 1/3
off if you buy a large quantity of it. (It goes fast when you start