Hi,
saw this interesting and inexpensive soldering clay hack on instagram…i havent tried it yet, but i will soon!…
using fullers earth (clump-able) cat litter as a soldering holding media
thought i would share…
julie
Hi,
saw this interesting and inexpensive soldering clay hack on instagram…i havent tried it yet, but i will soon!…
using fullers earth (clump-able) cat litter as a soldering holding media
thought i would share…
julie
That’s funny! In cold, snowy, frozen climates some people travel with a bag of kitty litter in their car for traction in case they get stuck in ice/snow. Who knew kitty litter is so versatile!
Thanks for sharing Julie!
Jeff
My cats produce lots of soggy wet litter every week. Now I have a potential use for it…Rob
Ewww! stinky! Lol