Hi, I’m new tpo the list and want to say I think this is a wonderful
forum. My partner has spoke very highly of this list… Anyone have
any experience in casting 22k gold? Does this follow the same rules
as 14 or 18 with perhaps a higher flask temperature? Can this even
be done? I have tried this and have some pitting
problems…thankyou. Debra

Hi Debra, Yes, Casting 22 k gold as well as any karat all the way to
24k can be done. It is all a matter of flask temperature and metal
temperature…Either your flask temp may be too hot (probably) or
your metal temperature. Daniel Grandi