Bronze wire, granules

the gas welding rod is bronze. 

Check the alloy content of any welding rod. In general, if they are
mainly copper and zinc, they’re actually brass, even they may be
called bronze on the packaging. If it’s mainly copper and tin, it’s a
true bronze.

Judy Bjorkman