Do any of the bronze pmc clays work well with enameling? Any special
instructions I should follow?

Thanks!

Do any of the bronze pmc clays work well with enameling? Any
special instructions I should follow? 

Not Bronze Clay, but you can enamel on Copper Clay, see the book by
Pam East on the topic. Yes, there are very special instructions in
how you fire the work for enameling. It’s all in her book.

Elaine
http://www.CreativeTextureTools.com

I’ve also seen enamelling done on steel clay. But it didn’t look
anything like it does on copper, silver or gold clays.

Barbara