the coating of boric acid protects the surface of the diamond from
oxygen not heat. It is the oxygen that is the cause of the daimond
"burning". Think of how the boric acid dip keeps your gold from
turning black during soldering. Again it is not he heat but the
introduction of oxygen to the unprotected surface that turns the
metal black, same with a diamond.