Hello Rob,
Did I miss the results on grinding the borax in a box to make flux? I can’t find it in the archives.
Sorry, got sidetracked. Will try today…Rob
I discovered that I had made up a solution of finely ground borax and water when we first had this discussion, but never tried it out. I tried it yesterday on a test piece of sterling silver and medium solder. It worked fine. Sorry for the delay…Rob