Watch Video:

Just an aside on this remember it must be ferretic stainless
materials- 361 and all those will not work you could use plastic
coated metal pins to stir up the non magnetics to prevent
dissimilliar metal contamination ?? but then SHAWN will have
experimented with something to over come this issue