DeDe have you had silver rings to size with a plating that
bubbles up when you solder and how can jewelers deal with this at
one time silver was just silver now it has plating on it and
makes it hard for the jeweler to do his work and keep the
customer happy well i need to get off my soap box!!! this is to
all the list thank jack
Dear Jack:
I never had that problem! The few times I have had a silver
piece plated, I already done all my solderng prior to the
plating… This bubbling problem sounds like a real b*#@%!!!