Hello,
No despite the florescent green Batterns doesn't contain fluorides. It is sodium borate (AKA Borax) and ammonium chloride which is where the "Self Pickling" attribute on the label comes from.
Not according this article where I found the answer James.
But for ones I believe you -))
Have fun and enjoy
Pedro