Hey Will, the craft store suggestion is a good lead. There’s a
plastic mesh “canvas” available that’s used with yarn (think large
cross-stich) for variouse craft projects. One of my teachers at GBC
cast it in silver with great success, though he did sprue the hell
out of it. Good luck!