CAUTION THIS COULD BE HAZARDOUS TO YOUR HEALTH!!!
Know that is out of the way. When I first started in this industry
(about 20 years ago) we used, hear comes the bad word, ASBESTOS. To this
day I still use it

I dont wnt to rain on your parade, but I’ve got to tell you that the
incubation period for asbestos caused lung cancer is 20 years !!
I’d suggest that you stop using it at once.