Hi All,

Can anyone working with Argentium tell me if improvements have been
made to the solders lately. I recall many complaints, some mine,
about ghosting and since my originial trials I have been using SS
solder on the Arg stock - - but would like to go back to the
Argentium solder at some point if it has been improved. ?