Thanks, Priscilla Fritsch, for referencing my article in Art Jewelry
Magazine. I think, (blowing own horn?) that it covered the topic
very thoroughly and the magazine did a terrific job of reproducing my
samples. The article is, thought, not about alternatives to using
LOS, but how to use it on sterling and fine silver and copper.