Jay some years ago I bought an airbrush specifically for blasting
media (you didn’t use sand, the media was finer) from Daniel Smith. I
don’t know if they still offer it. Here is their address,
www.danielsmith.com

I wouldn’t try my airbrush unless I didn’t care if I ruined it. I
would assume that the tips are different and very likely the tip
opening. Patti