Hi anyone heard of this?

935 sterling silver snake chains Pronice, German tarnish retardant
treatment, world patented nano technology.

Sold by Stones and Silver Australia.

Richard.


#2

I believe 935 is Argentium. At least that is how the Hallmark stamps
are sold

Lesley


#3
I believe 935 is Argentium. At least that is how the Hallmark
stamps are sold 

A&E are going to be selling Argentium :slight_smile: CIA