Hi I use the following 18ct white gold alloy which gives an
brilliant white gold colour - au75/pd15/ag5/cu5 that was
recommended by Magma Metal Recoveries. Theoretical and
practical info with regards to annealling 18ct white gold would
be = appreciated.

Thanks

Alan Rathbone


#2

Alan, when annealing white gold bring up to 1000Degrees and hold
for about 20 seconds at this color. Completely let this air cool
and pickle.

Good Luck